Originální abstrakt

Buckling resistance (including flexural buckling and lateral-torsional buckling) is major design parameter for many structural glass components. Buckling resistance is influenced by several parameters: boundary conditions, slenderness and initial imperfections. Initial imperfections, in particular initial geometrical out-of plane curvatures are very poorly presented in literature. In this paper measuring and determining of initial geometrical imperfections of fifteen specimens are presented. Measured specimens had the same dimensions but they had different composition – there are made from monolithic glass or laminated glass using PVB or EVA foil bonding together annealed glass panes or fully tempered glass panes. The shape of initial overall bow was measured using CARL ZEISS testing equipment. Information about initial curvature shapes and amplitudes are major conclusions resulting from statistical evaluation of tests.

Anglický abstrakt

Buckling resistance (including flexural buckling and lateral-torsional buckling) is major design parameter for many structural glass components. Buckling resistance is influenced by several parameters: boundary conditions, slenderness and initial imperfections. Initial imperfections, in particular initial geometrical out-of plane curvatures are very poorly presented in literature. In this paper measuring and determining of initial geometrical imperfections of fifteen specimens are presented. Measured specimens had the same dimensions but they had different composition – there are made from monolithic glass or laminated glass using PVB or EVA foil bonding together annealed glass panes or fully tempered glass panes. The shape of initial overall bow was measured using CARL ZEISS testing equipment. Information about initial curvature shapes and amplitudes are major conclusions resulting from statistical evaluation of tests.

Klíčová slova

Structural glass, initial geometrical imperfections, flexural buckling, normal distribution, log-normal distribution

Klíčová slova v angličtině

Structural glass, initial geometrical imperfections, flexural buckling, normal distribution, log-normal distribution

Autoři

PEŠEK, O.; MELCHER, J.

Rok RIV

2016

Vydáno

01.10.2015

Nakladatel

WSEAS - World Scientific and Engineering Academy and Society

ISSN

2224-3429

Periodikum

WSEAS Transactions on Applied and Theoretical Mechanics

Svazek

2015

Číslo

10

Stát

Bulharská republika

Strany od

253

Strany do

259

Strany počet

7

URL

BibTex

@article{BUT117896,
  author="Ondřej {Pešek} and Jindřich {Melcher}",
  title="Measuring and Evaluation of the Shape and Size of Initial Geometrical Imperfections of Structural Glass Members",
  journal="WSEAS Transactions on Applied and Theoretical Mechanics",
  year="2015",
  volume="2015",
  number="10",
  pages="253--259",
  issn="2224-3429",
  url="http://wseas.org/wseas/cms.action?id=10178"
}