Acoustic Testing of Reinforced Concrete Structure Corrosion

TIMČAKOVÁ-ŠAMÁRKOVÁ, K. CHOBOLA, Z. ŠTEFKOVÁ, D.

Originální název

Acoustic Testing of Reinforced Concrete Structure Corrosion

Anglický název

Acoustic Testing of Reinforced Concrete Structure Corrosion

Jazyk

en

Originální abstrakt

The paper deals with the study of dominant frequencies of an Impact-Echo method response signal obtained from a reinforced concrete beam with a steel rod diameter of 8 mm. Tension pulse was produced in the centre of the concrete beam and detected in opposite position of the concrete beam. Dominant frequencies of the response signal will be the main criterions for the reinforced concrete rebar corrosion progress. The article presents the results of measurements obtained after 24 months controlled degradation in aqueous NaCl solution.

Anglický abstrakt

The paper deals with the study of dominant frequencies of an Impact-Echo method response signal obtained from a reinforced concrete beam with a steel rod diameter of 8 mm. Tension pulse was produced in the centre of the concrete beam and detected in opposite position of the concrete beam. Dominant frequencies of the response signal will be the main criterions for the reinforced concrete rebar corrosion progress. The article presents the results of measurements obtained after 24 months controlled degradation in aqueous NaCl solution.

Dokumenty

BibTex


@inproceedings{BUT110191,
  author="Kristýna {Timčaková} and Zdeněk {Chobola} and Daniela {Kysilková}",
  title="Acoustic Testing of Reinforced Concrete Structure Corrosion",
  annote="The paper deals with the study of dominant frequencies of an Impact-Echo method response signal obtained from a reinforced concrete beam with a steel rod diameter of 8 mm. Tension pulse was produced in the centre of the concrete beam and detected in opposite position of the concrete beam. Dominant frequencies of the response signal will be the main criterions for the reinforced concrete rebar corrosion progress. The article presents the results of measurements obtained after 24 months controlled degradation in aqueous NaCl solution.",
  address="German Society for Non-Destructive Testing",
  booktitle="31st Conference of the European Working Group on Acoustic Emission (EWGAE)",
  chapter="110191",
  howpublished="electronic, physical medium",
  institution="German Society for Non-Destructive Testing",
  year="2014",
  month="september",
  pages="1--6",
  publisher="German Society for Non-Destructive Testing",
  type="conference paper"
}