Originální abstrakt

This paper presents the results of an experimental study with a focus placed on the long-term mechanical-, fracture- and fatigue analysis of mortar, in which natural aggregates (NA) were partially substituted with fine recycled concrete aggregates (RCA). Long-term tests were done at 28, 145 and 255 days under natural aging conditions. Fracture and fatigue experimental analysis took place for tensile mode I, which was enriched by fracture tests performed under a combination of tensile and shear load – mixed-mode I/II loading conditions. In total, four mixtures (reference and three with fine RCA) were tested to examine the influence of the aggregate replacement on the fracture and fatigue properties of the material. The experimental results showed that 25 % of replacement seems to be an optimum dosage of fine RCA, which improves both the fracture and fatigue properties of tested mixtures.

Anglický abstrakt

This paper presents the results of an experimental study with a focus placed on the long-term mechanical-, fracture- and fatigue analysis of mortar, in which natural aggregates (NA) were partially substituted with fine recycled concrete aggregates (RCA). Long-term tests were done at 28, 145 and 255 days under natural aging conditions. Fracture and fatigue experimental analysis took place for tensile mode I, which was enriched by fracture tests performed under a combination of tensile and shear load – mixed-mode I/II loading conditions. In total, four mixtures (reference and three with fine RCA) were tested to examine the influence of the aggregate replacement on the fracture and fatigue properties of the material. The experimental results showed that 25 % of replacement seems to be an optimum dosage of fine RCA, which improves both the fracture and fatigue properties of tested mixtures.

Klíčová slova

Mortar Recycled Concrete Aggregate Fatigue Fracture long-term behaviour

Klíčová slova v angličtině

Mortar Recycled Concrete Aggregate Fatigue Fracture long-term behaviour

Autoři

MIARKA, P.; ŠIMONOVÁ, H.; KUCHARCZYKOVÁ, B.; SEITL, S.; POLETANOVIC, B.; MERTA, I.

Rok RIV

2026

Vydáno

06.05.2025

Nakladatel

Elsevier

ISSN

0950-0618

Periodikum

Construction and Building Materials

Svazek

481

Číslo

1

Stát

Spojené království Velké Británie a Severního Irska

Strany počet

16

URL

Plný text v Digitální knihovně

BibTex

@article{BUT197857,
  author="Petr {Miarka} and Hana {Šimonová} and Barbara {Kucharczyková} and Stanislav {Seitl} and Bojan {Poletanovic} and Ildiko {Merta}",
  title="Optimisation of fine RCA content in mortar mixture based on the long-term fracture and fatigue tests",
  journal="Construction and Building Materials",
  year="2025",
  volume="481",
  number="1",
  pages="16",
  doi="10.1016/j.conbuildmat.2025.141371",
  issn="0950-0618",
  url="https://www.sciencedirect.com/science/article/pii/S0950061825015193?via%3Dihub#ack0005"
}